The NHT² is designed to provide low loads with depth measurements in the nanometer scale for the measurement of hardness, elastic modulus, creep, etc. The system can be used to characterize organic, inorganic, hard and soft materials.

With the unique top surface referencing technique, an indentation measurement can be made in less than 3 minutes without waiting for thermal stabilization.

 

Force:

Resolution: 0.01

Max force: 500 mN

Depth:

Resolution: 0.01 nm

Max. depth: 200

Load frame stiffness:

>> 107 N/m

International standards:

ISO 14577, ASTM E2546, etc.